## TL;DR

Researchers developed a flexible, biocompatible electrode using cellulose, PDMS, and glycerol for improved wearable biomedical devices.

## Contribution

A novel composite bioelectrode combining cellulose, PDMS, and glycerol was developed with enhanced conductivity and skin-conformability.

## Key findings

- The electrode showed low bulk resistance (0.658 kΩ) and high conductivity (0.0193 S m−1).
- It demonstrated a charge storage capacity of 4.626 mC m−2 and a low elastic Young modulus of 10.3 ± 5.4 kPa.
- ECG signals recorded with the electrode had a signal-to-noise ratio of 33.31 dB.

## Abstract

Flexible and biocompatible electrodes are crucial components in developing future wearable and implantable biomedical devices. In this work, a novel composite bioelectrode from cellulose, supported by polydimethylsiloxane (PDMS), and glycerol were developed. Cellulose, an abundant and biodegradable biopolymer, provides the conductivity, while PDMS provides the support and the mechanical elasticity. All together, they provide elasticity and skin-conformability. Glycerol was added in this work as it also acts as an ionic conductor and a plasticizer, thus, improving interfacial charge transfer and electrode hydration stability. The composite was fabricated by an easy polymerization and curing process. The morphological, electrochemical, and mechanical characteristics of the fabricated electrode were evaluated. Electrochemical impedance spectroscopy (EIS) and cyclic voltammetry (CV) showed low impedance, high conductivity, and stability. The electrochemical characteristics demonstrated the lowest bulk resistance of 0.658 kΩ, a conductivity of 0.0193 S m−1 and a charge storage capacity of 4.626 mC m−2. The ductile properties for the samples showed a low elastic Young modulus of 10.3 ± 5.4 kPa. Electroencephalograph (ECG) signal was recorded at a considerable good quality with SNR of 33.31 dB. Thus, the cellulose–PDMS–glycerol electrode material appears to offer a highly promising, green platform for the development of soft bioelectronics to be employed in real-time physiological signal monitoring.

Flexible and biocompatible electrodes are crucial components in developing future wearable and implantable biomedical devices.

## Linked entities

- **Chemicals:** glycerol (PubChem CID 753)

## Full-text entities

- **Chemicals:** Glycerol (MESH:D005990), PDMS (MESH:C013830), Cellulose (MESH:D002482)

## Full text

_Full body text omitted from this summary view._ Fetch the complete paper as Markdown: https://tomesphere.com/paper/PMC12273340/full.md

## Figures

8 figures with captions in the complete paper: https://tomesphere.com/paper/PMC12273340/full.md

## References

34 references — full list in the complete paper: https://tomesphere.com/paper/PMC12273340/full.md

---
Source: https://tomesphere.com/paper/PMC12273340