Scaling properties of pyrex and silicon surfaces blasted with sharp particles
Z. Moktadir, H. Wensink, M. Kraft

TL;DR
This study investigates the multifractal scaling properties of surfaces of Pyrex glass and silicon after blasting with alumina particles, revealing scale-dependent fracture and correlation effects.
Contribution
It is the first to analyze the multifractal properties of blasted brittle surfaces using MFDFA, showing independence from material and particle size.
Findings
Surfaces exhibit multifractal properties across scales.
Singularity spectrum is unaffected by material or particle size.
Fracture dominates at scales below 5 microns.
Abstract
The blasting of brittle materials with sharp particles is an important fabrication technology in many industrial processes. In particular, for micro-systems, it allows the production of devices with feature sizes down to few tens of microns. An important parameter of this process is the surface roughness of post-blasted surfaces. In this work the scaling properties of Pyrex glass and silicon surfaces after bombardment with alumina particles is investigated. The targets were bombarded at normal incidence using alumina particles with two different average sizes, and , respectively. This investigation indicates that the resulting surfaces have multifractal properties. Applying multifractal detrended fluctuation analysis (MFDFA) allowed us to determine the singularity spectrum of the surfaces. This spectrum did not depend on the target material or on the size of the…
Peer Reviews
No public reviews on file for this paper yet. If you reviewed it on a platform where reviews are public (OpenReview, ICLR, NeurIPS, ICML), you can paste yours below so the community can read it here.
Videos
No videos yet. Explain this paper in a talk, walkthrough, or lecture? Add one.
The reference list from the paper itself. Each links out to its DOI / PubMed record.
- 1Slikkerveer et al. (2000) P. Slikkerveer, P. Bouten, and F. de Haas, Sensors. and Actuators 85 , 296 (2000).
- 2Belloy et al. (1999) S. Belloy, E. Thurre, A. Walckiers, Sayah, and M. Gijs, Eurosensors XIII proceeding, the Hague, Holland p. 827 (1999).
- 3Veenstra et al. (2001) T. T. Veenstra, J. W. Berenschot, J. G. E. Gardeniers, R. G. P. Sanders, M. C. Elwenspoek, and A. van den Berg, J. Electrochem. Soc. 148 , G 68 (2001).
- 4Schlautmann et al. (2001) S. Schlautmann, H. Wensink, R. M. Schasfoort, M. Elwenspoek, and A. V. D. Berg, J. Micromech. Microeng. 11 , 386 (2001).
- 5Slikkerveer et al. (1998) P. J. Slikkerveer, P. Bouten, F. in’t Veld, and H. Scholen, Wear 217 , 237 (1998).
- 6Chen et al. (2005) X. Chen, J. W. Hutchinson, and A. G. Evans, J. Am. Ceram. Soc. 88 , 1233 (2005).
- 7Lawn and Fuller (1975) B. R. Lawn and E. R. Fuller, J. Mater. Sci. 10 , 2016 (1975).
- 8Marshall et al. (1982) D. B. Marshall, B. R. Lawn, and A. G. Evans, J. Am. Ceram. Soc. 65 , 561 (1982).